Product/Mold Description
What are the main causes of die drool on plastic extrusion dies?
Die drool and other die flow irregularities are most often caused by internal
die surfaces that are scratched or pitted, or that have poor plating quality.
What are your ideas for optimizing sleeving applications?
For sleeving applications, you want to establish the correct drawdown
ratio and draw ratio balance for the material being extruded. Next, you
want to have a land that is appropriate for the die gap. For pressure
extrusion, you need an opening that is sufficient for the core to pass
through, but not large enough to allow leaking inside the tip.
Generally speaking, sleeving tooling improves wall thickness control,
and pressure tooling is better for faster line speeds.
Product Name
|
UPVC Plastic Window Extruder Mold
|
Material
|
3Cr17, 3Cr17MoNiV, DIN1.2316 or Negotiable
|
Color
|
Silvery
|
Mould cavity
|
One or Multi-Cavity
|
Feature
|
High Polished Surface, Stable Discharging, Soft-hard, Surface Layer, Cladding
|
Test
|
Mould will be tested to get the satisfy sample before delivery
|
Sample
|
Sample will be arranged by express for customer approval
|
Service
|
Provide complete set of formulation, technology and perfect after sale service
|
Lead time
|
30-35days
|
Package & delivery time
|
Poly wood case for exporting, each mould will be cleaned before packing.
|
Remark:
|
If you are interesting in mould and plastic prodcuts, welcome you provide us the details of the product material , size , weight ect, better 2D and 3D drawing. Welcome you to visit us.
|